Mixing cement, water, and aggregates (such as sand, gravel, or crushed stone) to create a durable and strong building...
PCC is laid in layers with a thickness of 4 Inch of (1:4:8) under the raft using OP Cement and Local Sand with the use of mechanical vibrators for complete compaction. Hand compaction may be necessary in certain areas to ensure complete compaction and proper alignment within the mold. Compaction should be completed within thirty minutes of water addition to prevent premature setting. Mixing of Plain...